HomeM16×1.5 › M16×1.5 torque spec

M16×1.5 Torque Spec

Calculated preload torque by grade, plus what actually changes the number.

M16×1.5 · 8.8 · dry threads 233 N·m 172 lb-ft · targets 72.8 kN clamp load (75% of proof)

By grade

GradeDry (N·m)Lubed (N·m)Dry (lb-ft)Clamp loadUltimate tensile
4.6
Low-carbon steel, general purpose
90.367.766.628.2 kN66.9 kN
8.8
Medium-carbon, quenched & tempered — the default structural grade
23317517272.8 kN133.8 kN
10.9
Alloy steel, Q&T — high strength
333250246104.1 kN173.9 kN
12.9
Alloy steel, Q&T — highest common grade (socket head cap screws)
389292287121.7 kN204 kN
A2-70
304 stainless, cold worked
18113513356.4 kN117.1 kN

Why lubrication changes everything

Roughly 90% of the torque you apply is consumed by friction — under the head and in the threads. Only about 10% becomes useful bolt stretch. That means the friction coefficient, not the bolt, sets the relationship between torque and clamp load. Here is the same M16×1.5 8.8 fastener under different conditions:

Thread conditionNut factor KTorque for same preload
Plain / as-received, dry0.20233 N·m
Zinc plated, dry0.22256 N·m
Black oxide, lightly oiled0.18210 N·m
Machine oil on threads0.15175 N·m
Molybdenum disulfide / anti-seize0.12140 N·m
Waxed or PTFE coated0.10116 N·m
Torquing a lubricated bolt to the dry spec overloads it — the 116 N·m row and the 233 N·m row produce the same clamp load. Apply the dry number to a waxed fastener and you are at roughly twice the intended preload, which for a 8.8 is past yield.

Assumptions behind these numbers

T = K × D × F with K = 0.20, F = 0.75 × proof load, and proof load = tensile stress area (167.25 mm²) × the grade's proof strength. This is a general-engineering starting point for a reusable steel-on-steel joint. It is not a substitute for a manufacturer's torque sequence on an engine, a suspension component, a pressure vessel or any structural connection.

Related for M16×1.5