1-1/2-6 UNC · Grade 5 · dry threads 1950 lb-ft 2644 N·m · targets 77991 lb clamp load (75% of proof)

By grade

GradeDry (lb-ft)Lubed (lb-ft)Dry (N·m)Clamp loadUltimate tensile
Grade 2
Low/medium carbon steel, unmarked head
869652117934,779 lb103,988 lb
Grade 5
Medium carbon Q&T, 3 radial head marks
19501462264477,991 lb168,630 lb
Grade 8
Medium carbon alloy Q&T, 6 radial head marks
316223714287126,472 lb210,787 lb
18-8 SS
304/18-8 stainless
1054790142942,157 lb105,393 lb

Why lubrication changes everything

Roughly 90% of the torque you apply is consumed by friction — under the head and in the threads. Only about 10% becomes useful bolt stretch. That means the friction coefficient, not the bolt, sets the relationship between torque and clamp load. Here is the same 1-1/2-6 UNC Grade 5 fastener under different conditions:

Thread conditionNut factor KTorque for same preload
Plain / as-received, dry0.201950 lb-ft
Zinc plated, dry0.222145 lb-ft
Black oxide, lightly oiled0.181755 lb-ft
Machine oil on threads0.151462 lb-ft
Molybdenum disulfide / anti-seize0.121170 lb-ft
Waxed or PTFE coated0.10975 lb-ft
Torquing a lubricated bolt to the dry spec overloads it — the 975 lb-ft row and the 1950 lb-ft row produce the same clamp load. Apply the dry number to a waxed fastener and you are at roughly twice the intended preload, which for a Grade 5 is past yield.

Assumptions behind these numbers

T = K × D × F with K = 0.20, F = 0.75 × proof load, and proof load = tensile stress area (1.40525 in²) × the grade's proof strength. This is a general-engineering starting point for a reusable steel-on-steel joint. It is not a substitute for a manufacturer's torque sequence on an engine, a suspension component, a pressure vessel or any structural connection.